| Grain structure |
Rough |
| Hardness Vickers |
~ 200 HV |
| Temperature * |
< 400° C (752°
F) |
| Welding/soldering |
Good/very good
|
| Sharp bending |
Possible |
| Edge sharpness |
Poor |
| Mostly used for |
Sieves or high
temp. |
* For a harder nickel with finer grain structure
additives are used in the plating chemistry          
< back |
|